About
WAAM3D
Wire bAsed Additive Manufacturing for everyone
WAAM3D Limited
5 Thornton Chase
Milton Keynes
MK14 6FD United Kingdom
Useful Links
About us
About us
Why WAAM?
Industries
Our team
Software
WAAMPlanner
WAAMKeys
WAAMCtrl
WAAMDisplay
Systems
Turnkey systems
Our end-effector
Parts
Print With us
Material properties
Services
Projects
MultiFUN
Wires
Aluminium 2319
Aluminium Magnesium Scandium
Titanium 64 / Standard
Titanium 64 / Straight
Blog
WAAM3D Limited is incorporated
WAAM3D joins the Eagle Lab
Series A completed
MULTI-FUN project aims to enable multi-materials metal additive manufacturing for complex 3D parts without size constraints
Careers
About us
About us
Why WAAM?
Industries
Our team
Software
WAAMPlanner
WAAMKeys
WAAMCtrl
WAAMDisplay
Systems
Turnkey systems
Our end-effector
Parts
Print With us
Material properties
Services
Projects
MultiFUN
Wires
Aluminium 2319
Aluminium Magnesium Scandium
Titanium 64 / Standard
Titanium 64 / Straight
Blog
WAAM3D Limited is incorporated
WAAM3D joins the Eagle Lab
Series A completed
MULTI-FUN project aims to enable multi-materials metal additive manufacturing for complex 3D parts without size constraints
Careers
Superalloy 718 as-deposited
Material description
Enter material content
Nickel-based superalloy
Two letter code
Enter two letter element's code to be displayed
Ni
Material code
Enter material code identifier
Ni718
UTL H (MPa)
Enter Ultimate Tensile Strength H in MPa
810
UTL V (MPa)
Enter Ultimate Tensile Strength V in MPa
750
PS H (MPa)
Enter Proof Strength H in MPa
530
PS V (MPa)
Enter Proof Strength V in MPa
810
E H (%)
Enter Elongation H in %
34
E V (%)
Enter Elongation V in %
28